[3A01]Electrochemical reduction of simulated vitrified waste glass in molten salt for separation and recovery of LLFPs

*Yumi Katasho1, Kouji Yasuda2,3, Toshiyuki Nohira1 (1. Institute of Advanced Energy, Kyoto Univ., 2. Agency for Health, Safety and Environment, Kyoto Univ., 3. Graduate School of Energy Science, Kyoto Univ.)

[3A02]Investigation of Cs Leaching Behaviour from spent Zeolite Solidified using Borate Glass

*Akane Usui1, Aiki Watanabe1, Tsuyoshi Arai2 (1. Shibaura Institute of Technology Graduate School, 2. Shibaura Institute of Technology)

[3A03]Leaching behavior of constituent elements from vitrified waste containing spent zeolite used in the contaminated water treatment

*Aiki Watanabe1, Akane Usui1, Tsuyoshi Arai2 (1. Shibaura Institute of technology Graduate School , 2. Shibaura Institute of technology)

[3A04]Search of vitrification matrix with high-loading capacitychange of chemical durability with monovalent and divalent metal content

*Ryo Souma1, Katsushige Komatsu1, Shigeru Yamamoto1, Akihiro Yamada1, Jun Matsuoka1, Kouhei Oowaku2, Norio Kanehira2 (1. The university of shiga prefecture, 2. Japan Nuclear Fuel Limited)