[3I13]NaFeO2からなるナトリウムイオン電池負極の創製
*Hiroyasu Watanabe1,2, Hiroyuki Usui2,4, Yasuhiro Domi2,4, Kurumi Uetake3,4, Takahiro Nishida3,4, Haruki Kurokawa1, Hiroki Takahashi2,4 (1. Toda Kogyo Corp., 2. Graduate School of Engineering, Tottori Univ., 3. Graduate School of Sustainability Science, Tottori Univ., 4. Center for Research on GSC, Tottori Univ.)
[3I14]Sn4P3/Sbコンポジットからなる電極のナトリウムイオン電池負極特性
*Atsuki Teramae1,3, Hiroyuki Usui2,3, Yasuhiro Domi2,3, Naoto Oishi4, Noriko Nitta4, Hiroki Sakaguchi2,3 (1. Graduate School of Sustainability Science, Tottori Univ., 2. Graduate School of Engineering, Tottori Univ., 3. Center for Research on GSC, Tottori Univ., 4. School of Environ. Sci. and Eng., Kochi Univ. of Tech.)
[3I15]二価アルコール添加した水系電解液を用いたNaTi2(PO4)3の負極特性
*Ayuko Kitajou1 (1. Yamaguchi University)
[3I16]SIB用負極材料としてのターフェニルトリカルボン酸塩異性体の合成及び電気化学的特性評価