[3MH13]機械的摂動場における電極の微細構造変化のin-situ測定:SEM×DICによる複合解析

*Yuki Tanaka1 (1. Nitto Analytical Techno-center Co.,Ltd.)

[3MH14]Structure Evolution of NCM Cathodes under Fast Charge/Discharge Conditions

*Chunzhen Yang1, Yuying Zhang1 (1. Sun Yat-sen University (China))

[3MH15]Gr系負極を用いたLIBの部分充放電による非破壊劣化解析

*Keisuke Matsuda1, Kumi Shono1, Yo Kobayashi1, Junpei Yamanaka1 (1. Tokyo Electric Power Company Holdings, Inc.)

[3MH16]SPAN正極を用いたリチウムー硫黄二次電池”Li–SPAN”のセル安全性

*Kenji Kakiage1, Hiromi Sato1, Yuji Morishima1, Anne Dailly2, Fang Dai2, Insun Yoon2, Yifan Zhao2, Yuta Ikeuchi3, Takashi Mukai4, Shunsuke Saito5, Kohei Umetsu6, Ayako Abe6, Hideaki Sasaki1, Xiaoxiao Yang1, Naoto Yamashita4, Taichi Sakamoto4, Hiroyuki Ozaki3, Shingo Tanaka3, Kentaro Kuratani 3, Toru Yano1 (1. ADEKA CORPORATION, 2. General Motors Company, 3. National Institute of Advanced Industrial Science and Technology, 4. ATTACCATO Limited Liability Company, 5. URUTAMA.INC, 6. ENAX,Inc.)