Session Details
Evaluation of agglomerated ore
Thu. Mar 12, 2026 10:00 AM - 11:20 AM JST
Thu. Mar 12, 2026 1:00 AM - 2:20 AM UTC
Thu. Mar 12, 2026 1:00 AM - 2:20 AM UTC
Room1(No.8 Bldg. 2F 8201)
足立毅郎 [神鋼]
[17]In-situ observation of cracks formation in iron ore pellets under hydrogen reduction conditions
〇Koki Momma, Taichi Murakami (Tohoku Univ.)
[18]Evaluation of the reducibility of low-grade iron ore pellets
〇Gin'ichiro Sato, Yuji Ewami, Tetsuya Yamamoto (JFE)
[19]Effect of distribution of MgO source on sinter microstructure and low-temperature reduction disintegration
〇Mizuki Yamakawa1, Taichi Murakami1, Masaru Matsumura2 (1.Tohoku Univ., 2.Nippon Steel)
[20]3D microstructure analysis of reduced sinter ore using X-ray CT
〇Toru Takayama, Reiko Murao, Satoshi Yamada (Nippon Steel)