[J5]Ultrafine-grain refinement makes Ti-O alloy ductile at 77 K

*Yan Chong1,2,3, Reza Gholizadeh1, Ruopeng Zhang3, Andy Minor3, Nobuhiro Tsuji1,2 (1. Department of Materials Science and Engineering, Kyoto University)

Keywords:

titanium,oxygen interstitial,grain size,mechanical property

We explored the effects of grain refinement(by severe plastic deformation and annealing) on the low temperature tensile properties and deformation behaviors of Ti-O alloys