Session Details
[G]High Temperature Oxidation and Corrosion (1)
Wed. Mar 8, 2023 1:30 PM - 5:00 PM JST
Wed. Mar 8, 2023 4:30 AM - 8:00 AM UTC
Wed. Mar 8, 2023 4:30 AM - 8:00 AM UTC
Rm. C Rm.166,2nd Flr.,Buld.No.1
Chair:Yen-Ling Kuo(Nagaoka University of Technology), Takumi Nishimoto
※表示の講演時間には質疑応答時間も含みます。
(質疑応答時間5分、基調講演と招待講演は5~10分)
(質疑応答時間5分、基調講演と招待講演は5~10分)
[12]Grain boundary oxygen diffusion in polycrystalline Al2O3 determined by oxidation rate of AlN/Al2O3 composites
*Phanuwat Khlaisongkhram1, Yen-Ling Kuo1, Makoto Nanko1 (1. Nagaoka University of Technology)
[13]Strength Recovery Behavior of Ni/Al2O3 Self-healing Ceramics
during High Temperature Oxidation
*Daisuke MARUOKA1, Takehiro HASHIMOTO2, Taichi MURAKAMI1, Eiki KASAI1 (1. Graduate School of Environmental Studies, Tohoku University)
[14]Effect of oxygen partial pressure on oxidation behavior of SiC dispersed Yttrium Silicate composites by oxidation in water vapor
*Thi Huong NGUYEN1, Yen Ling KUO1, Makoto NANKO1 (1. Nagaoka University of Technology)
[15]Influences of composition control and Nb addition on oxidation behavior of Ti2AlC ceramics
*Naoya Yamaguchi1, Ryutaro Sugai1, Dąbek Jaroslav2, Brylewski Tomasz2, Yen-Ling Kuo1, Makoto Nanko1 (1. Nagaoka University of Technology, 2. AGH University of Science and Technology)
break
[16]Boiling Water Reactor Severe Accident Conditions Evaluation of Steam Oxidation Reaction of SUS304-B₄C Melt Solidified Products
*KOSUKE INOUE1, AYUMI ITOH2, SHINTARO YASUI2,3, YOSHINAO KOBAYASHI1,2 (1. School of Material and Chemical Technology, Tokyo Institute of Technology, 2. Laboratory for Zero-Carbon Energy, Tokyo Institute of Technology, 3. Laboratory for Materials and Structures, Tokyo Institute of Technology)
[17]High temperature corrosion behavior of martensitic stainless steel in water vapor containing HCl at 350℃
*Sakka TAKERU1, Hayashi Shigenari2, Yoneda Suzue2, Yamamoto Ryotaro3 (1. Graduate School of Engineering, Hokkaido University, 2. Faculty School of Engineering, Hokkaido University, 3. Ebara Corporation)
[18]The effect of Cr content on oxidation behavior and the microstructure of Al2O3 scale on Al-containing ferritic stainless steels for SOFCs interconnect
*shouh heng Tai1, Febry Muhammad2, Shigenari Hayashi3 (1. Hokkaido Univ., 2. JFE Steel Corp., 3. Hokkaido Univ.)
[19]Co-doping Y/Hf on the oxidation behavior of alumina-forming Co-based oxide dispersion strengthened superalloys
*Hao YU1, Sosuke Kondo1, Yasuyuki Ogino1, Ryuta Kasada1 (1. Tohoku Uni.)
break
[20]Interactive Effects of Nb and Ti on Cr2O3 Scale Formation on Austenitic Steels
*Ryo Tatsushima1, Shigenari Hayashi2, Suzue Yoneda2 (1. Hokkaido Univ.(Master), 2. Hokkaido Univ.)
[21]Study on pre-oxidation method of thermal barrier coatings
*Masahiro NEGAMI1,2, Kohei KYUMA2, Makoto AZUMA2, Tomoki TANIGUCHI2, Yoko YAMABE-MITARAI1 (1. The Univ. of Tokyo, 2. Kawasaki Heavy Industries)
[22]In-situ observation of oxidation behavior of Fe-Cr alloys in CO2
*Miremu Niimi1, Mitsutoshi Ueda2 (1. Tokyo Tech, 2. Tokyo Tech)
[23]Improvement of removability of oxide scale formed on steel by adding SiO2
*Aya HARASHIMA1 (1. Nippon Steel)