[P129]Effect of sintering modes and number of coating cycles on synthesizing porous aluminum utilizing aluminum dross
○Thi Xuan Mai Nong1, Takahiro SUZUMURA2, Yen-Ling KUO1, Makoto NANKO1 (1. Nagaoka Univ. of Technol., 2. SUZUMURA Co., Ltd.)
Keywords:
Porous ceramic,Aluminum dross,Recyling
Using considerably at 400°C for burning sponge temperature and at 1300°C sintering temperature with multiple layers shows the high structural stable ceramic foam.