Session Details
Hydrogen embrittlement 4
Mon. Mar 10, 2025 10:30 AM - 11:50 AM JST
Mon. Mar 10, 2025 1:30 AM - 2:50 AM UTC
Mon. Mar 10, 2025 1:30 AM - 2:50 AM UTC
Room9(Bldg.1 2F 210)
河盛誠 [神鋼]
[149]Hydrogen trapping behavior of Mo carbides in Mo-added steel
○Shunsuke Taniguchi, Miyuri Kameya, Yukiko Kobayashi, Kazuma Ito, Shingo Yamasaki (Nippon Steel)
[150]Atomic-scale observation of hydrogen trapping sites in heavily drawn pearlitic steels
○Jun Takahashi1, Kazuto Kawakami2 (1.Nippon Steel, 2.Nippon Steel Technology)
[151]Hydrogen embrittlement evaluation of drawn pearlitic steel wire by in-situ miniature tensile test in hydrogen-plasma scanning electron microscope
○Kota Tomatsu1, Takahiro Chiba1, Tetsushi Chida1, Tomohiko Omura1, Akimitsu Hatta2 (1.Nippon Steel, 2.Kochi Univ. of Tech.)
[152]Effects of Si, Cr, and Mo solid solution elements on the equilibrium hydrogen content in martensitic steels
○Ryota Nomura1, Kenichi Takai1, Tomohiko Omura2 (1.Sophia Univ., 2.Nippon Steel)