富松宏太 [日本製鉄]

[158]Tensile properties of SUS316L in hydrogen environment at low temperatures

Tatsumi Takeda1, Motoaki Morita1, Hayato Terada2, Kentaro Wada2, Uchino Takashi2, Yoshinori Ono2 (1.TUMSAT, 2.NIMS)

[159]Effect of hydrogen on tensile properties of Fe-36wt%Ni alloy at cryogenic temperatures

Taiki Maeda1, Fugao Wei1, Yoshinori Ono2, Kentaro Wada2, Masayuki Komatsu2 (1.Nippon Yakin Kogyo, 2.NIMS)

[160]Evaluation on hydrogen embrittlement of ultrafine grained SUS316Lsteel by 0.3mm thin wall hollow high pressure hydrogen low temperature tensile test

Shiro Torizuka1, Atsushi Ito1, Takafumi Komatsu2, Ryota Okitsu1, Taiga Mizuno1, Kaito Sonoda1 (1.Univ. of Hyogo, 2.Komatsu Seiki)

[161]Evaluation on hydrogen embrittlement of a heavily cold worked ultralow carbon steel by 0.3mm thin wall hollow high pressure hydrogen low temperature tensile test