[20p-B202-14]Fabrication of symmetric [010]-tilt grain boundaries of Fe(Se,Te)
〇Kazumasa Iida1,6, Yoshihiro Yamauchi2, Takafumi Hatano2,6, Jens Haenisch3, Zimeng Guo4,6, Hongye Gao4, Shinnosuke Tokuta5,6, Haoshan Shi4, Satoshi Hata4,6, Akiyasu Yamamoto5,6, Hiroshi Ikuta2 (1.Nihon Univ., 2.Nagoya Univ., 3.Karlsruhe Inst. of Tech., 4.Kyushu Univ., 5.Tokyo Univ. of Agricult. & Tech., 6.JST CREST)
Keywords:
Iron-based superconductor,grain boundary,critical current
We fabricated [010]-tilt roof-type grain boundaries in the iron-based superconductor Fe(Se,Te). The critical current density Jc between the grains (i.e., inter-grain Jc) was almost the same as that within the grains up to a grain boundary angle of 9º. This means that there is no weak link up to this grain boundary angle.