Presentation Information

[Material-02]Development of New Slurry Material for Airport Pavement Surfaces

*BINHUI WANG1, YUJI SESHITA1, TOMIO HIRAOKA1 (1. NICHIREKI GROUP CO., LTD. (Japan))

Keywords:

Slurry,Airport pavement,Simulation,Durability,Set time,Follow-up survey

Slurry materials, such as micro-surfacing and slurry seal, are recognized as effective means for maintaining and extending the service life of road pavements. In Japan, beyond road maintenance, there is a growing demand for lifespan-extension techniques for airport pavements. Therefore, we have developed a new slurry material to withstand aircraft loads, addressing two key challenges. First, it's difficult to obtain testing machines which can conduct real aircraft's amount of load. We proposed simulating the cumulative effect of load instead of the real amount of load. Among existing road pavement testing equipment, many examine structural changes in pavement layers under wheel loads, while few verify the strength of surface treatment materials themselves or their adhesion to the pavement. Our available wear tester, which evaluates materials by tire rotation on specimens, was identified as suitable. Using impulse (force x time) per unit area as a wear index, we successfully simulated cumulative aircraft wheel load effects. This method is applicable to various loads and fields. The second challenge was improving early-stage durability to meet short traffic-opening times while ensuring workability within a constrained curing period (approximately 5.5 hours). This was addressed by adding a polar polymer to the asphalt, which secured a set time of over 5 minutes and reduced early wear loss in the laboratory evaluation using aforementioned wear tester to 12g. This represents a more than tenfold improvement in early-stage wear resistance compared to conventional products (>180g). In addition, developed dedicated application machinery Trial application on an airport runway using this system yielded a satisfactory finish within the specified curing time with no early wear or peeling. While laboratory simulation indicated the developed material would wear out completely in 2 years and 3 months, field tracking after the same period confirmed the material remained largely intact, demonstrating superior wear resistance.