[Data_Collection-31]Optimizing Hot Mix Asphalt Macrotexture at the Mix Design Stage

*Stephen Goodman1 (1. Goodman Pavement and Materials Engineering Inc. (Canada))

Keywords:

Friction,Macrotexture,Hot Mix Asphalt,Road Safety,Superpave

Historically in North America, roadway pavement friction and macrotexture have not been evaluated after placement as a performance requirement, let alone at the mix design stage. With a greater focus on roadway safety in recent years, the US Federal Highway Administration (FHWA) has identified Pavement Friction Management (PFM) as a proven safety countermeasure capable of providing immediate and direct reduction in roadway crashes and injuries. The success of a PFM program requires collection and monitoring of continuous pavement friction and macrotexture data. The ability to estimate and optimize these properties at the mix design stage will allow road agencies to cost effectively evaluate their materials in the laboratory prior to placement on the road. In 2006, the Author introduced a method for estimating final Hot Mix Asphalt (HMA) macrotexture in the field by evaluating Superpave gyratory specimens in the laboratory – the first known use of this technique. In addition, preliminary models were developed to estimate macrotexture based on mix properties such as gradation, Voids in the Mineral Aggregate (VMA), and bulk relative density – thereby presenting the opportunity for modifying macrotexture as a mix design parameter in a similar way to other volumetric properties. This paper reviews the original Goodman models, as well as review and extension of the research by others to date. A recalibration of the models is presented - moving from Mean Texture Depth (MTD) from the sand patch test to Mean Profile Depth (MPD) from laser scanning. Application to a recent airport paving project is also presented. In this case, the airport authority specified a minimum macrotexture value that was not achieved in the field with the dense-graded HMA mixture. Use of the models during mix design, as well as testing of the gyratory specimens, would have identified the issue and allowed adjustments to meet the specification.