Presentation Information

[NpVBMPAo-05]Development of Low Carbon Semi-flexible Pavement using CO2-based Recycled Material

*MUHAMAD AFIF BIN OSMAN1, Masahiko Iwama1, Kenichi Yasuhisa2, Sachiko Hayashiguchi2, Yuta Itoh2 (1. NIPPO Corporation (Japan), 2. Sumitomo Osaka Cement Co., Ltd (Japan))

Keywords:

Semi-flexible Pavement,Artificial Limestone,CO2,Capture,Fixation

In recent years, increased concerns about global warming and climate change have made it desirable for all industries to tackle environmental issues worldwide. This problem is especially crucial for the transportation industry, where carbon dioxide (CO2) has been emitted throughout the vehicle’s operational life. Therefore, it is also vital for the paving industry, where CO2 is directly associated with the construction and maintenance of road surfaces. Meanwhile, to challenge this issue from the perspective of resource circulation, artificial limestone produced by recycling CO2 and waste concrete has recently been developed in the cement and concrete sector. The use of artificial limestone might be advantageous to reduce CO2 emissions because CO2 is captured and fixed during the recycling process. In addition, the application of the limestone as semi-flexible paving material has the potential to achieve carbon neutrality in the future, because it does not require the use of reinforcing bars that corrode during neutralization. Thus, developing semi-flexible pavements using artificial limestone is worthwhile, as the capture and fixation of CO2 is expected during construction and service. This paper describes the development of lower carbon semi-flexible pavement using CO2-based recycled materials and its application in a trial. Through its in-service performance, the following conclusions are drawn in this study. With respect to mechanical performance, laboratory results show that the developed material meets standard requirements, in terms of flexure and compression strength. The results also provide that the developed pavement performed better than that of conventional pavement in plastic flow resistance. Regarding workability, the field trial demonstrates that the developed material is workable, because cores extracted from the field prove that the developed pavement has high filling rate, compared to that of conventional pavement. In addition, no significant changes in skid resistance and rut depth have been observed in the developed pavement. The developed pavement exhibits greater carbonation depth in carbonation acceleration tests. Consequently, it demonstrates higher CO2 absorption performance compared to conventional pavement, making it an environmentally friendly pavement.