[2K14]Study on vitrification plan of high level liquid waste in the TVF(10) Discharging behavior for platinum group elements for the new glass melter

*Yusuke Aoyama1, Masaya Tone1, Daiki Shiramizu1, Nanako Katsuoka1, Koshi Miyata1, Shigeki Hukuda1, Hikaru Ohtaka1, Hidekazu Kobayashi1, Akira Kodaka1 (1. JAEA)

Keywords:

TVF,TVF's 3rd glass melter,Vitrification,Platinum group elements,XRF

In the new glass melter (the 3rd melter) at the Tokai Vitrification Facility (TVF), the bottom shape of the melter was changed from the square pyramid of the existing melter (the 2nd melter) to a cone to improve ability to discharge platinum group elements. To confirm the effect of the improvement, operational test using non-radioactive simulant of liquid waste containing platinum group elements was carried out. Discharging behavior of platinum group elements was evaluated in comparison with the 2nd melter.