[P176]Effect of third element additions on the oxide scale formation behavior of ZrSi2

*Keigo OSEKI1, Nobuaki SEKIDO2, Kyosuke YOSHIMI2 (1. Tohoku University, 2. Tohoku University)

[P177]Micro-electrochemical analysis of the role of Ti-addition in pitting resistance of ferritic stainless steels

*Kaito Takeuchi1, Izumi Muto2, shuji Nishida3, Masashi Nishimoto2, Yu Sugawara2 (1. Tohoku Univ., 2. Tohoku Univ., 3. JFE Steel Corporation)

[P178]Fabrication and analysis for corrosion behavior of Iron-based high-entropy alloys
containing Tantalum and Niobium

*Toshimasa Ishizawa1, Izumi Muto2, Masashi Nishimoto2, Yu Sugawara2 (1. Tohuku Univ. (student), 2. Tohoku Univ.)

[P179]Investigation of corrosion resistance of 3D printer molding materials with different stacking methods in SUS316L steel.

*Kenta ODA1, Masahiro KAIDO3, Ryoutaro YAMAMOTO3, Manabu NOGUCHI3, Masahiko HATAKEYAMA2, Satoshi SUNADA2 (1. 富山大理工(院生)、2. 富山大、3. 荏原製作所)

[P180]Inhibitory effect of copper oxide formation via submerged photosynthesis of crystallites by He+ ion irradiation

*Yu SATO1, Yuki NAKAGAWA2, Tamaki SHIBAYAMA2 (1. 北大工(院生)、2. 北大工)

[P181]Corrosion Behavior of Stainless Steel in Stress Loading Environment

*Ryota KIKUTI1, Yuta Yagi, Ryouji Suzuki, Kazuhiko Noda (1. Shibaura Institute of Technology)

[P182]Electrochemical Behavior of Peeling Plated Film Platinized Titanium Electrode

*Keigo HATTA1, Yuta YAGI, Kazuhiko NODA (1. Shibaura Institute of Technology Graduate School)

[P183]Corrosion Behavior of Zinc Rich Paint Coated Pure Iron

*JUNQING BAO1, RYOJI SUZUKI2,3, YUTA YAGI2,4, KAZUHIKO NODA2 (1. Dept. of Regional Environment Systems, Shibaura Institute of Technology, 2. Faculty of Engineering, Shibaura Institute of Technology, 3. Japan Power Engineering and Inspection Corporation, 4. Nakabohtec Corrosion Protecting Co., LTD.)

[P184]Two-step plasma nitriding using Ti-Al combination screen

*Ryusei Kajimoto1, Yasuhiro Hosiyama1, Tomoki Maruoka2 (1. Kansai University, 2. Kyoto Municipal Institute of Industrial Technology and Culture)

[P185]Structural Characterization of TiO2 Films Deposited by Glancing-angle Sputtering

*CHEN YUSOU1, Inoue Yasushi2, Takai Osamu3 (1. Chiba Institute of Technology, 2. Chiba Institute of Technology, 3. Kanto Gakuin University)

[P186]Appearance of strong electron correlation by forced substitution of other element in transition metal nitride CrN

*Takumi SUGAI1, Tsuneo SUZUKI1 (1. Nagaoka Univ. Tech)

[P188]Electrodeposition of Bi-Sb-Te Thermoelectric Material in Ethylene Glycol Non-aqueous solution

*MASAMORI AKIGUCHI1, HIROAKI YAMAMOTO2, AI NOZAKI2, MASAO MORISHITA2 (1. University of Hyogo(graduate student), 2. University of Hyogo)

[P189]Fabrication of electrodeposited Zn alloys with high strength for biodegradable implants

Ryusei ARAUCHI1, Hiroki KOTO2, *Yorinobu TAKIGAWA3 (1. Osaka Prefecture Univ., 2. Osaka Prefecture Univ. (Present: DAIHATSU MOTOR CO.), 3. Osaka Metropolitan Univ.)

[P190]Mechanism of hydrogenation of alkynes by Heusler alloy catalysts

*Takayuki KOJIMA1, Shinpei FUJII2, Satoshi KAMEOKA3 (1. Faculty of Textile Science and Technology, Shinshu University, 2. Graduate School of Science and Engineering, Kagoshima University, 3. Institute of Multidisciplinary Research for Advanced Materials, Tohoku University)

[P191]Decomposition of Rhodamine 6G over Tungsten Oxide Photocatalysts and Microstructure Observation by TEM

*Yasuhiro Shiratsuchi1, Tamaki Shibayama2, Yuki Nakagawa2 (1. 北海道大工学院、2. 北海道大工学研究院)