講演情報

[Recycle-12]Evaluation of cracking resistance across a wide temperature range for repeatedly recycled asphalt binders and asphalt mixtures

*THANH NHAT TRAN1, HIDEYUKI ANDO1, TSUYOSHI HYAKUTAKE1, IWAO SASAKI1, HIROYUKI NITTA1 (1. Public Works Research Institute (Japan))

キーワード:

repeated recycling、cracking resistance、RAP、asphalt binder、asphalt mixture

In Japan, pavement rehabilitation has been carried out for many years, and the use of repeatedly recycled asphalt mixtures and the proportion of reclaimed asphalt pavement (RAP) are expected to increase. As a result, repeated recycling increases binder stiffness, which may accelerate the deterioration of legacy asphalt on aggregates and thereby reduce the cracking resistance of RAP asphalt mixtures. The authors assessed the low-temperature cracking resistance of asphalt binders subjected to repeated recycling and identified a strong correlation with the high-temperature crack resistance of RAP mixtures at high-temperature. Nevertheless, it is essential to evaluate cracking resistance of asphalt binder and asphalt mixtures across a wide temperature range.This study aimed to evaluate the cracking resistance of asphalt binders subjected to repeated recycling and the RAP mixtures incorporating them across a broad temperature range, from high to low. The present study used two types of rejuvenators: one rich in aromatics and the other rich in saturates. The accelerated aging of asphalt was conducted using the Thin Film Oven Test and the Pressure Aging Vessel test. For the asphalt mixtures, the Cantabro test was conducted at high temperature, and indirect tensile (IDT) test was performed at intermediate temperature. For the binders, bending beam rheometer (BBR) test was conducted in the low-temperature range, and dynamic shear rheometer (DSR) test was performed from low to intermediate temperature.The results indicated that an increased number of recycling cycles using a saturate-rich rejuvenator may decrease the cracking resistance of RAP asphalt mixtures across high, intermediate, and low temperature ranges. In addition, DSR results, which can be obtained with fewer specimens, exhibited a strong correlation with BBR results. This finding indicates that the DSR test has potential applicability for evaluating the low-temperature cracking resistance of repeatedly recycled asphalt. Furthermore, the cracking resistance of repeatedly recycled asphalt mixtures can be assessed at intermediate temperature using a simple IDT test, which exhibited strong correlations with Cantabro results at high temperatures and BBR results at low temperatures. These findings suggest that the IDT test may improve the efficiency of asphalt mixtures tests in the evaluation of repeated recycling.