Presentation Information

[PS-11]Beyond Initial Oxidation: Long-Term Internal Corrosion Behavior of AISI 347H at 700 °C in Humid Environments

*Hooman Karimi Abadeh1, Hampus Lindmark1, Tobias Mattison2, Torbjörn Jonsson1, Jesper Liske1 (1. Department of Chemistry and Chemical Engineering, Chalmers University of Technology (Sweden), 2. Department of Space, Earth and Environment, Chalmers University of Technology (Sweden))

Keywords:

High Temperature Corrosion,Stainless Steel,Chromia,Healing Layer,Long term


Comment